Nanhaiya Non-Intermeshing Parallel Twin Screw Barrel wis dirancang kanthi teliti kanggo garis ekstrusi PVC, PE, lan WPC. Wiwit diadegake minangka produsen tong minyak sekrup profesional ing China ing taun 2014, Nanhaiya terus-terusan menehi prioritas kanggo ngirim solusi ekstrusi sing paling apik sing ora mung regane kompetitif nanging uga njamin kinerja sing stabil. Nalika pelanggan mutusake kanggo njupuk Barel Screw Kembar Paralel Non-Intermeshing saka Nanhaiya, dheweke nandur modal ing produk sing misuwur amarga keseimbangan torsi sing apik, efisiensi output sing luar biasa, lan umur operasional sing luwih dawa. Atribut kasebut ndadekake pilihan kanggo klien internasional kanggo ngupayakake peralatan ekstrusi sing bisa dipercaya lan berkinerja tinggi.

Nanhaiya Non-Intermeshing parallel twin screw barel mlaku podo karo nanging ora intermesh, ngurangi geser nalika njaga transportasi materi sing konsisten. Konfigurasi iki nyegah akumulasi panas sing berlebihan lan njaga sifat materi. Laras digawe saka baja paduan premium, diantrekake karo karbida nikel-tungsten, lan mesin presisi kanggo njamin toleransi sing ketat. Cocog kanggo senyawa polimer, produksi WPC, lan bahan sing mbutuhake penanganan sing ati-ati sajrone ekstrusi.

Parameter Produk (Spesifikasi)

Bahan

38CrMoAlA

Kekerasan Perlakuan Panas

HB260-320

Kekerasan Nitriding

HV950-1000

Kedalaman Nitriding

0,50-0,70 mm

Nitriding Brittleness

≤kelas 1

Kasar

Ra0.4

Straightness Screw

0,015 mm

Chrome Plating atose

HV≥950HV

Ketebalan Chrome

0,05-0,10 mm

Kekerasan Bimetal

HRC60-65

Kedalaman Bimetal

2.0-3.0mm

Fitur Product lan Aplikasi

Barel non-intermeshing digunakake ing ngendi geser kurang lan campuran alus dibutuhake. Padha becik kanggo profil PVC, decking WPC, lan termoplastik sensitif. Laras ngidini rasio pangisi sing luwih dhuwur nalika njaga integritas materi lan kualitas produk sing konsisten.

Non-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw Barrel

Rincian Produksi

Saben laras sekrup kembar Nanhaiya paralel ngalami mesin CNC majeng lan penggilingan presisi. Lumahing wis rampung pangilon kanggo nyilikake gesekan lan nambah aliran plastik. Penerbangan meneng wis hardened dening nitriding utawa lapisan alloy bimetallic kanggo stabilitas long-term.

Non-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw BarrelNon-Intermeshing Parallel Twin Screw Barrel
Kirim Pitakonan
Info kontak
Sugeng rawuh ing situs web kita! Kanggo pitakon babagan produk utawa dhaptar rega, tinggalake email sampeyan lan kita bakal hubungi sajrone 24 jam.
X
Kita nggunakake cookie kanggo menehi pengalaman browsing sing luwih apik, nganalisa lalu lintas situs lan nggawe konten pribadi. Kanthi nggunakake situs iki, sampeyan setuju kanggo nggunakake cookie. Kebijakan Privasi
nolakNampa